82-5160-121-01
Male
Right angle
Crimping
Crimping
H155
Availability: | |
---|---|
Quantity: | |
Materials&Electroplating | |
Conduct | Brass/ Silver Plating |
Insulator | PTFE |
Body | Brass /Ternary |
Other Parts | Brass/ Nickel Plating |
Electric Performance | |
Impedance | 50 OHMS |
Frequency Range | 0-3GHz |
VSWR | ≤1.30 |
Rating Voltage | 500V |
Environmental | |
Temperature Rating | -65°C to +165°C |
Corrosion (Salt Spray) | MIL-STD-202, Method 101, Condition B |
Vibration | MIL-STD-202, Method 204, Condition D, 20 Gs |
Shock | MIL-STD-202, Method 213, Condition I, 100 Gs |
Thermal Shock | MIL-STD-202, Method 107. Cond. B, -65°C to +125°C |
Moisture Resistance | MIL-STD-202, Method 106, Less Step 7B |
Materials&Electroplating | |
Conduct | Brass/ Silver Plating |
Insulator | PTFE |
Body | Brass /Ternary |
Other Parts | Brass/ Nickel Plating |
Electric Performance | |
Impedance | 50 OHMS |
Frequency Range | 0-3GHz |
VSWR | ≤1.30 |
Rating Voltage | 500V |
Environmental | |
Temperature Rating | -65°C to +165°C |
Corrosion (Salt Spray) | MIL-STD-202, Method 101, Condition B |
Vibration | MIL-STD-202, Method 204, Condition D, 20 Gs |
Shock | MIL-STD-202, Method 213, Condition I, 100 Gs |
Thermal Shock | MIL-STD-202, Method 107. Cond. B, -65°C to +125°C |
Moisture Resistance | MIL-STD-202, Method 106, Less Step 7B |